You can be light with the brush on your second application to minimise the brush marks if its an issue. Remember also your backing layer, wether it is putty or wet laid glass fibre, should be going on when the gel is still tacky. When at that stage, rolling flat any fibreglass will likely squish most of the brush marks anyway.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|