Windsurfing mast


Author
Message
kaso
kaso
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 21

Hi

I need to repair this windsurfing mast, see attached pictures.

The problem here is the downward pressure making the fibre going apart. My guess it that the pressure is around 200-300kg.

Any idea how to fix this? Which fiberorientation could best take up the pressure?



Attachments
2014-07-13 10.55.42.jpg (290 views, 1.00 MB)
2014-07-13 16.57.38.jpg (276 views, 1.00 MB)
2014-07-13 16.57.38.jpg (292 views, 1.00 MB)
Edited 11 Years Ago by kaso
Reply
kaso
kaso
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 21
Thanks for your replies, I have now bonded two rings on mast and it seems like it will work. 
 