Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
mould section joins
mould section joins
Post Reply
Like
3
mould section joins
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Ian974
Ian974
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 92
Hi everyone.
I've been reasonably successful with building the mould for my front bodywork (which has gone very well for a first attempt, picture is as it came off the bodywork).
The moulds look horrible there but the paint that came off cleaned up fairly easily and I'm in the process of cleaning up the moulds, flanges and making any repairs before going on to making the carbon version.
However one bit I'm not too happy with is that the joins between the mould sections are a bit rough. Is there any way of improving or filling these up prior to making the new bodywork? It'll need work done afterwards anyway but just seeing if there is a way to improve them at all. I'll see if I can get a more representative photo later today.
Cheers!
Attachments
2014-04-12 17.42.56.jpg
(
515 views,
1.00 MB
)
Edited
11 Years Ago by
Ian974
Reply
Like
3
Reply
ajb100
ajb100
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Are you making the piece in grp or cf?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
mould section joins
Ian974
-
11 Years Ago
Your mould joins should be all sweet and flush if the original pattern flanging was set up and done...
Fasta
-
11 Years Ago
Sorry, the flanges themselves all match up ok, but the joins on the mould surface are a bit uneven,...
Ian974
-
11 Years Ago
Can you not just re-fillet the mould sections before layup?
FLD
-
11 Years Ago
I just like to understand what you have done. So when you set up your original splitting flange...
Fasta
-
11 Years Ago
Yeah, that's it. I tried smoothing the fillets down fairly small, but not enough. My 20-20 hindsight...
Ian974
-
11 Years Ago
Yeah, normally your temp flange will be fitted/butted close to your body/pattern/plug and then any...
Fasta
-
11 Years Ago
Are you making the piece in grp or cf?
ajb100
-
11 Years Ago
That more or less explains what I have, though unfortunately I am looking at doing resin infusion...
Ian974
-
11 Years Ago
Plasitcene/wax is really about the only option I can think of, it wont stick to anything so no need...
Fasta
-
11 Years Ago
Not managed to get any other photos yet,been a few other jobs I've needed to get done on the car. If...
Ian974
-
11 Years Ago
[quote][b]Ian974 (19/07/2014)[/b][hr]Not managed to get any other photos yet,been a few other jobs...
Fasta
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search