Hi, I'm making a pattern for a boot spoiler, the way i was going to do it was to laser cut profile templates from 3mm hardboard (see attachment), space them at 50mm intervals on the boot lid, fill the gaps with pattern making low density PU foam blocks hot melt glued into the gaps.
next sand down to the profiles, skim with filler, pattern coat etc.

can anyone see any reason why this wouldn't work ok?
Attachments
IMG_2608.jpg (592 views, 1.00 MB)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
That will work absolutely fine mate, that's almost exactly how I built mine Smile 
Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K




It worked out quite well,
Here's the plug in pattern coat primer











http://www.talkcomposites.com/Uploads/Images/7271a2e6-2868-4099-86a5-0bed.JPG