Resins, Gelcoats and Pigments
»
Paper Catch Pot Liners on Website
Paper Catch Pot Liners on Website
Post Reply
Like
9
Paper Catch Pot Liners on Website
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
James Stefanou
James Stefanou
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 8
Hi,
I was wondering if this profile is the only one that you produce, as I have a pressure pot setup with a very specific internal geometry.
If not, are you able to forward me on to the company that produce these liners for you?
Kind Regards,
James Stefanou
+61 407 856 684
Tags
Catch-pot
disposable
liner
paper
resin
Reply
Like
9
Reply
James Stefanou
James Stefanou
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 8
Thanks for the responses guys, I was after a more repeatable, process-friendly solution though.
Is your pressure vessel built to suit a particular liner or?
How do you ensure all resin is utilized in an infusion, without large wastage? We're based in Australia and i'm finding it very hard to source a local supplier to provide this type of product, and am happy to consider overseas supply.
Cheers,
James
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Paper Catch Pot Liners on Website
James Stefanou
-
12 Years Ago
They are an off the shelf paper cup which we source from various suppliers. You should be able to...
Warren (Staff)
-
12 Years Ago
You don't have to use a cup if they don't fit, could also just line it with some vacuum bag or...
Hanaldo
-
12 Years Ago
Thanks for the responses guys, I was after a more repeatable, process-friendly solution though. Is...
James Stefanou
-
12 Years Ago
As long as the cup fits you will be fine. Plan your resin feed and distribution to help avoid...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search