Hi all, after some help please…

I am making a "mould" but without an original part, its a simple item so I am making from foam core and was going to "paint it" using Uni Mould obviously using the catalyst and using the MW agent stuff, so I am mixing it as you would for doing a mould repair so it dries out.

My problem is I know if I paint brush this on to the flat surface and then look to flat it off afterwards, most of my time will be spent just rubbing out the brush stroke marks, I believe the Uni Mould is to thick to spray on so how can you apply this giving the flattest finish??

I am thinking of using a paint brush to apply it and then using a roller to get a better flat finish prior to rubbing it down. Has anyone done this before and can pass on their advice please?

Cheers,
Lee.
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
He did say he would be using the wax additive so it cures hard. 

OP, it might help if you detail what you are trying to achieve, but I really do think using the Unimould is the hardest way to go about it. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Ah, didn't spot that....
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search