Hi all, after some help please…

I am making a "mould" but without an original part, its a simple item so I am making from foam core and was going to "paint it" using Uni Mould obviously using the catalyst and using the MW agent stuff, so I am mixing it as you would for doing a mould repair so it dries out.

My problem is I know if I paint brush this on to the flat surface and then look to flat it off afterwards, most of my time will be spent just rubbing out the brush stroke marks, I believe the Uni Mould is to thick to spray on so how can you apply this giving the flattest finish??

I am thinking of using a paint brush to apply it and then using a roller to get a better flat finish prior to rubbing it down. Has anyone done this before and can pass on their advice please?

Cheers,
Lee.
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
My first question on using the unimould gelcoat would be can it fully cure when exposed to an "air" environment? Most gels won't (well poly gel won't) I've not tried a vinylester  gel before so don't know the ins and outs of it.

If it's "just a simple channel" then why not just make a male (or female) box out of MDF or HDPE?