posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 49
Is the high temp base coat need to be cure the same way as the high temp epoxy? If so how how long do I have to post cure it?
Reply
Like
7
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Yes, to acheive its high HDT (Heat Distortion Temperature) the
High Temperature Epoxy Skinning Basecoat
would also need to be post-cured at elevated temperatures. The post cure schedule is the same as that for the
High Temperature Epoxy Laminating Resin
. You'll find the recommended post-cure schedule on the
Datasheet for the High Temperature Epoxy
.
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
basecoat
cycle
high
post cure
temperature
Reply
Like
9
fx3861
fx3861
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 49
ok as for the HT epoxy do i have to post cure for every coating or just the ending coating as it never stated on it..
Reply
Like
12
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Do all your post-curing at the end when you have laminated all the layers of resin on BUT BEFORE YOU START FLATTING IT. This will ensure that if the resin sags into the weave during post curing then you can flat this out afterwards.
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search