By fx3861 - 3/28/2012 4:13:58 AM
Is the high temp base coat need to be cure the same way as the high temp epoxy? If so how how long do I have to post cure it?
|
By Matt (Staff) - 5/5/2012 10:31:17 AM
Do all your post-curing at the end when you have laminated all the layers of resin on BUT BEFORE YOU START FLATTING IT. This will ensure that if the resin sags into the weave during post curing then you can flat this out afterwards.
|
|