Hi All,

I have a question about Gel coats.

I currently have a tooling for a sports performance canoe and I am sourcing any thoughts on stenciling designs in different colours prior to laying up.

Could a clear gelcoat be sprayed locally and a decal/ sticker laid over the clear before the complete hull colour being applied?

Cheers 
Replies
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hello imig,
 I would recommend just adding decals when craftis finished,,  yes you could  spray a local clear and then put coloured gel over the top, but I think you would get a colour  variation where you sprayed the clear,  
Kind Regards
The Fibreglass King


Imiq Paddle Sports
Imiq Paddle Sports
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 8, Visits: 63
Thanks Fibreglass King,

I appreciate your response.

If I was to go down the, clear gelcoat locally route, would there be any seperation/ de-lam issues where the two gelcoats start & finish?

Cheers

Imiq Paddle Sports 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search