Hello,

As I'm new in carbon fiber, I'm wondering about the ratio 100:30 which is printed on the containers , what does mean, if there is any example please?
Reply
HTFL
HTFL
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Hi,




Also suppose you have 5 kg Epoxy. Then the Resin would be 5kg x 0.77 = 3.85 kg and the hardener would be 5kg x 0.23 = 1.15 kg.