If you are not sure, just keep it simple and mix in batches of 100g of resin. That way for every 100g of resin, you need 30g of hardener. Simple enough to do in your head and be confident youve got it right.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|