benet
benet
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 59,
Visits: 373
So, i accidentally grabbed a small bottle of resin IN2 instead if hardener (SLOW) when my hardener bottle ran out and completed the mix with more resin. Ive ended up with a mold with resin in it thats only got half the hardener in it it should have. Shall i bin it all now or is it worth waiting? and waiting ....
Thanks
Ben
Reply
Like
2
Replies
brainfart
brainfart
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 198,
Visits: 1.4K
The resin will eventually solidify, but its thermal and mechanical properties will suffer.
Reply
Like
2
benet
benet
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 373
4 days later and the resin is still not cured. tacky, thick , but not at all cured.. Binned - lesson learned i hope.,
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
wrong mix - will it ever cure ?
benet
-
11 Years Ago
I hate to say it but probably not, epoxy needs a very specific range of ratio's to actually cure....
ChrisR
-
11 Years Ago
no, its still all pretty runny ! lol.. lesson learned. i was too used to my rein being in big pots...
benet
-
11 Years Ago
The resin will eventually solidify, but its thermal and mechanical properties will suffer.
brainfart
-
11 Years Ago
4 days later and the resin is still not cured. tacky, thick , but not at all cured.. Binned - lesson...
benet
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search