Hey all,

Due to a lack of any available epoxy tooling gelcoats where I live, I have started making my own using laminating resin and a variety of fillers and additives. I like to add a black pigment, as the black makes it really easy to find low spots and polish to a great shine, however my issue is that most of the fillers I use are a white powder, so instead of a nice solid black gelcoat I end up with a sort of gunmetal grey. 

I have managed to get away with using that colour, but I would like to find out if it is possible for me to create my gelcoats with the solid black that I'm after. I don't want to add too much pigment obviously, and anything beyond 2% doesn't seem to do much regardless. So, how do proper tooling gelcoats like the Unimould system obtain such a nice black colour?
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Not sure if I understand your question the right way but when I buy a gelcoat it is transparant then I add 15% of coloured pigment (liquid) and I get a full cover coloured gelcoat/resin 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Hanaldo - 11 Years Ago
matthieutje65 - 11 Years Ago
ajb100 - 11 Years Ago
Devin Wang - 11 Years Ago
matthieutje65 - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
brainfart - 11 Years Ago
ajb100 - 11 Years Ago
brainfart - 11 Years Ago
Hanaldo - 11 Years Ago
Dravis - 11 Years Ago
Hanaldo - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search