BlackNDecker
BlackNDecker
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 92,
Visits: 251
In an attempt to refine my technique, I am going to scale back and try a smaller project. This is a solid plug that will eventually become the lower plenum of my intake manifold. I made it by making a mold of the aluminum flange and building a foam core. I added tubular elbow and a throttle body mounting plate. The whole thing has been sprayed with primer and sanded smooth. It's not glass smooth but pretty smooth nonetheless.
Here are some pics. This intake manifold is a multipiece design...the lower section I've made will replace this section:
Not perfect...but I can't tell you how elated I was to actually make a successful mold!!!
Fast forward...this is what it looks like and how it will mount to my intake manifold:
Is it even possible to mold this? There are some really tight crevices that worry me. I am also unsure about molding the cylindrical tube.
Reply
Like
3
Reply
BlackNDecker
BlackNDecker
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 92,
Visits: 251
Finished up the other half of the plenum. Very happy with how it turned out...I'm refining the technique and its coming out better and better. I spent alot if time making sure there was no bridging at the lower flange.
It's gonna take a lot of trimming but this is how it's gonna look:
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How would you mold this...?
BlackNDecker
-
11 Years Ago
I would do it as a 2 piece mould, straight down the middle. The tube looks like it is offset a...
Hanaldo
-
11 Years Ago
Made some slow progress...flanged up with fillet wax:...
BlackNDecker
-
11 Years Ago
Backed it with 2 layers of 3/4 oz and 2 layers of 1.5 oz....
BlackNDecker
-
11 Years Ago
Progress! [IMG]http://i736.photobucket.com/albums/xx10/swolehead/null_zps21a5fa4a.jpg[/IMG]
BlackNDecker
-
11 Years Ago
How do you effectively seal the joins in your molds for vacuum infusion?
TargaMustang
-
11 Years Ago
Envelope bag. Can also just run some mastic tape along outside of the flanges where they join...
Hanaldo
-
11 Years Ago
I won't be able to mold this as a one piece unit. The shape is too complex. It will have to be two...
BlackNDecker
-
11 Years Ago
[quote][b]BlackNDecker (19/06/2014)[/b][hr]I won't be able to mold this as a one piece unit. The...
Hanaldo
-
11 Years Ago
Will the two halves be glued edge to edge, or is there a flat mating surface? In the former case,...
brainfart
-
11 Years Ago
[quote][b]brainfart (19/06/2014)[/b][hr]Will the two halves be glued edge to edge, or is there a...
BlackNDecker
-
11 Years Ago
http://www.rc-network.de/magazin/artikel_06/art_06-020/art_020-01.html Unfortunately this is in...
brainfart
-
11 Years Ago
[img]http://www.rc-network.de/magazin/artikel_06/art_06-020/bilder/k_leiste6.jpg[/img] You could...
brainfart
-
11 Years Ago
I don't have the proper vocabulary to describe all this since obviously English is not my native...
brainfart
-
11 Years Ago
Thanks guys...I really appreciate the advice! Hanaldo, would you happen to have a link to your...
BlackNDecker
-
11 Years Ago
Sorry mate, I meant my thread about my OEM replica wing. You posted in it asking how I joined the...
Hanaldo
-
11 Years Ago
Indeed...the alligator skinning is only on the flange. Finished the mold this afternoon. How long...
BlackNDecker
-
11 Years Ago
I knocked out the mold of the lower plenum this weekend...it is now ready for business:)...
BlackNDecker
-
11 Years Ago
Looks good mate, came out well :)
Hanaldo
-
11 Years Ago
Very nice and very interested in how this is progressing.
BoostSamurai
-
11 Years Ago
Things are progressing right along. I spent the last week sanding and waxing the mold. On a whim, I...
BlackNDecker
-
11 Years Ago
That's an expensive through-bag connector to destroy with infusion... Get yourself some silicone or...
Hanaldo
-
11 Years Ago
Yeah, I will get some silicone connectors...I just had some of these lying around. I'm using flow...
BlackNDecker
-
11 Years Ago
looks good so far cant wait to see it pulled
kidpaint
-
11 Years Ago
Sorry...forgot to update this thread. The first part had some bridging but it was just a test run so...
BlackNDecker
-
11 Years Ago
Finished up the other half of the plenum. Very happy with how it turned out...I'm refining the...
BlackNDecker
-
11 Years Ago
Looks good. cant wait to see it finished!
kidpaint
-
11 Years Ago
So I changed up the technique to try and eliminate the labor intensive process of vacuum infusing...
BlackNDecker
-
11 Years Ago
So the pre-preg was a semi-success. I was able to mold the manifold 1-piece with minimal trimming...
BlackNDecker
-
11 Years Ago
Did you run the vac bag through the middle of the mould so the bag was pushing against the carbon?...
ajb100
-
11 Years Ago
[quote][b]ajb100 (11/08/2014)[/b][hr]Did you run the vac bag through the middle of the mould so the...
BlackNDecker
-
11 Years Ago
I have read your post and looked at the pictures. It does not say or show if you bagged through the...
Brian_s
-
11 Years Ago
I did bag it and pulled the bag through the cavity. It's irrelevant though because the bag burned...
BlackNDecker
-
11 Years Ago
It's not surprising the bag burned through, your oven isn't really big enough for that size part and...
ChrisR
-
11 Years Ago
I read that it had burned through. But you had not mentioned that the bag went through the inside as...
Brian_s
-
11 Years Ago
Did you post cure your mould before you put the release on for the pre preg ? You need to burn the...
f1rob
-
11 Years Ago
Shouldn't you be copying the internal surface of the original manifold and not the external surface?...
asmasm
-
11 Years Ago
[quote][b]asmasm (13/08/2014)[/b][hr]Shouldn't you be copying the internal surface of the original...
BlackNDecker
-
11 Years Ago
Edit: Never mind, I see you are only doing half the intake in carbon and leaving the OEM runner...
asmasm
-
11 Years Ago
[IMG]http://i736.photobucket.com/albums/xx10/swolehead/null_zps7a93a000.jpg[/IMG]...
BlackNDecker
-
11 Years Ago
Is that the infusion item or the pre-preg? Looks like you've put a layer of resin over the top?
Hanaldo
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search