Is it possible to use ABS plastic structure as a core material for CFRP laminating?

For example,
1, I 3D-print some  core material structure  which is made of ABS plastic.
2, Next I laminate some CFRP on the ABS core structure,then I use vacuum bag or something to cure.

If it is possible,
I think I can make unique shape parts(curved tube,for example) in short time.
but I wonder that the ABS core structure separates from CFRP skin when the part is under stress.
then ABS core structure is useless as a core material.

Thanks,
Reply
hietaka
hietaka
Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)
Group: Forum Members
Posts: 14, Visits: 169
>>Matthieu san,

Thanks for responding!

well, I believe that 3D printed parts will be useful in some situation.
so I will try!