			            Is it possible to use ABS plastic structure as a core material for CFRP laminating?
 For example,
 1, I 3D-print some  core material structure  which is made of ABS plastic.
 2, Next I laminate some CFRP on the ABS core structure,then I use vacuum bag or something to cure.
 
 If it is possible,
 I think I can make unique shape parts(curved tube,for example) in short time.
 but I wonder that the ABS core structure separates from CFRP skin when the part is under stress.
 then ABS core structure is useless as a core material.
 
 Thanks,
 
 |