Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
vacuum pump size
vacuum pump size
Post Reply
Like
3
vacuum pump size
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
bewbzout
bewbzout
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 46
Is there such a thing as too big of a vacuum pump? I am looking at buying a 8cfm 2 stage pump. Thoughts? Bigger? I plan on building a hood or bonnet for you boys across the water. Thanks
Reply
Like
3
Reply
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Not really, CFM is just how quickly it moves the air. You need a pump that can pull 99% Vacuum, it doesn't matter how quickly it does it. So in most cases you will be paying for a big pump that you don't really need. And in fact if all you are doing is Vacuum bagging or infusion, then the smaller pumps can actually be better because you will have time to position the bag nicely etc.
The only time a big pump would really be useful is for degassing, as it can empty the chamber quicker. That can still be done using a smaller pump it might just take awhile. I use a 2cfm pump for all my work and it works fine.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
vacuum pump size
bewbzout
-
11 Years Ago
Not really, CFM is just how quickly it moves the air. You need a pump that can pull 99% Vacuum, it...
Hanaldo
-
11 Years Ago
Ok yea that is food for thought. I guess I just go overkill on everything I do lol.
bewbzout
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search