Been given a brand new material to test which gives a perfect pin hole free finish....  I have to admit until now the best material has been VTF261 (Easypreg by another name) but the cost has driven me to use other materials. If you buy VTF direct you have to order 50sq/m as a minimum order so buying Easypreg is the only other alternative source for the material.. So at a reasonable quantity you are looking at just under £83 per meter to buy.. The material I have just tried will be cheaper and after testing it this week works every bit as well as VTF (easypreg).

I have a contract to make dive tank covers I had to use a material I was supplied which I knew would need to be lacquered. I tried the new material and was impressed with the results.. I have used another material and had parts 95% as good as VTF and perfectly acceptable to my usual customers as it is out of the mould. But this was flawless....

Once I have been given permission to let people know about it I will. But for now it is a material that is close to launch and not yet available.


Here are two covers I made. One with each material..

This one is a PRF RF464. This is fresh material which arrived this week...
 

This is the new material which arrived this week too.....


Sorry the photos are not the best as these are just from my phone's camera.... 



No pin holes at all.... The down side is the customers supplied mould is now the weak link for a great part... He is now having a new mould made which will be finished to a proper gloss and any imperfections will be removed..
Replies
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
Great parts!

please keep posted on the material? any sneak info you could provide such as if it might be avail in USA/Canada?
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
20_rc51_00 (30/03/2014)
Great parts!

please keep posted on the material? any sneak info you could provide such as if it might be avail in USA/Canada?


It does have a good out life so I am sure they could ship to the USA/Canadia... If you wanted them to... 
So far it has been perfect but I am not sure if the way I have had to work with a similar spec material has helped as I do put my breather stack down in a very specific way as well as cooking with specific steps in the way I ramp up the temp and dwell at a lower temperature similar to VTF but with a couple of changes. 

I will get some better photos today....
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
morepower - 11 Years Ago
20_rc51_00 - 11 Years Ago
morepower - 11 Years Ago
morepower - 11 Years Ago
Hanaldo - 11 Years Ago
morepower - 11 Years Ago
Hanaldo - 11 Years Ago
morepower - 11 Years Ago
tack talk - 11 Years Ago
morepower - 11 Years Ago
morepower - 11 Years Ago
carbonfibreworks - 11 Years Ago
tha_pop - 11 Years Ago
     Nice
ekomposit.dk - 11 Years Ago
tack talk - 11 Years Ago
morepower - 11 Years Ago
Hanaldo - 11 Years Ago
tha_pop - 11 Years Ago
morepower - 11 Years Ago
tha_pop - 11 Years Ago
tha_pop - 11 Years Ago
Fasta - 11 Years Ago
morepower - 11 Years Ago
     SHD ???
f1rob - 11 Years Ago
f1rob - 10 Years Ago
morepower - 10 Years Ago
20_rc51_00 - 11 Years Ago
morepower - 11 Years Ago
20_rc51_00 - 11 Years Ago
morepower - 11 Years Ago
cpkielycua - 11 Years Ago
20_rc51_00 - 11 Years Ago
20_rc51_00 - 11 Years Ago
morepower - 11 Years Ago
                 send me a pm too if possible :)
matthieutje65 - 11 Years Ago
tack talk - 11 Years Ago
morepower - 11 Years Ago
morepower - 11 Years Ago
morepower - 11 Years Ago
     those look nice!
20_rc51_00 - 11 Years Ago
gp composites - 11 Years Ago
Shaneer22 - 11 Years Ago
morepower - 11 Years Ago
cpkielycua - 11 Years Ago
Steyrn - 11 Years Ago
TopComposite - 11 Years Ago
morepower - 10 Years Ago
JRT - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search