Hey all,



Thought I would just post up the latest project I have been working on; can always do with being told how to do it better.



So the project is a 4" intake pipe for my R34 Skyline. I wanted to attempt making something from scratch, and given I only had a 3" intake pipe previously I couldn't use that to make a mould for this one. So I started off by using the centreline of my current intake pipe to make a 3D drawing with the dimensions and cross-sections that I needed. I also added 100mm to the straight section on the end, as I wanted to move the air filter further away from the exhaust manifold:













From there I was able to print out the cross-sections I needed, and transfer them to some 3mm balsa wood:

1978698_10151893592392541_851850552_n.jp


Which allowed me to create the skeleton structure of the part:

13258_10151893592592541_220306668_n.jpg

1969113_10151893592482541_2049077103_n.j

I then needed to in-fill the gaps, so I made some low density polyurethane foam using a 2-part pour in place system. With this being the product. I made 4 of these 'blocks'.

1939973_10151864422067541_1752244226_n.j

Then I used this foam to fill in the 'body' of my part:

1800297_10151893592332541_2015330979_n.j

10001515_10151893592277541_1181756648_n.


Trimmed and sanded down to size, and voila!

1002650_10151893592227541_412985007_n.jp

1507560_10151893592162541_1344011204_n.j

From here, I filled and sealed the part with epoxy resin filled with microballoons:

1625670_10151893592107541_491525122_n.jp

1743691_10151893592047541_1909517110_n.j

Then used a stainless steel and fibreglass reinforced body filler to fill in the big gaps:

1896929_10151893591957541_1177675812_n.j

Flattened it down: 

1798764_10151893591882541_853076597_n.jp

10001573_10151893591832541_647456446_n.j

Then used the same filler to cover the whole thing, so I could fill in any low spots in the foam:

1975156_10151893591732541_1009989563_n.j

Sanded it down again, then trial fitted it in the car:

1621730_10151893591622541_381023724_n.jp

1965001_10151893591557541_1479490234_n.j

1907562_10151893591442541_1212210863_n.j

Perfect fitment to the mm!

10006383_10151893591587541_810697348_n.j


Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
What do you think of this as an option Warren? If I drilled a hole in the pipe, then stuck this through the hole and used the weld on lip to bond it in? 

http://speedflowdirect.com.au/itemdetailspage/20387

The only thing I don't like about it is it looks like by the time I have drilled a big enough hole to fit the threads through, I won't have much area left for the lip to bond onto? 
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hanaldo (29/03/2014)
What do you think of this as an option Warren? If I drilled a hole in the pipe, then stuck this through the hole and used the weld on lip to bond it in? 

http://speedflowdirect.com.au/itemdetailspage/20387

The only thing I don't like about it is it looks like by the time I have drilled a big enough hole to fit the threads through, I won't have much area left for the lip to bond onto? 


I can see where your going. Could you not just bond it on the outside. That way you could drill a smaller hole. You could even take the adhesive over the lip for a stronger mechanical bond?

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
carbonfibreworks - 11 Years Ago
matthieutje65 - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
Toffee - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
Hanaldo - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
wildcard - 11 Years Ago
Nick10 - 11 Years Ago
Hanaldo - 11 Years Ago
asmasm - 11 Years Ago
Hanaldo - 11 Years Ago
Jadleybray - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search