Hi guys, need sum help here. 
Got to make this spoiler. Its 3 part. 2 side panels and 1 blade ( main spoiler bit)
The side panels got to a be certain thickness to be rigid. 
This needs to ne frp not carbon. So im planning to make with wovenglass and soric lantor and do a resin infusion. 
My question is how i can seal the edge of the blades? They are pretty easy panels to get the molds.
Kinda confused as how to make make molds and how do i make the edges sealed and smooth?
Or any other way to make this panels?
Cheers

Attachments
image.jpg (656 views, 107.00 KB)
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Sorry, read blade as the end plates!

Havnt got a huge amount of experience with wings, but I've used the permabond adhesive from EC to join mine together.

F3 wings which use a support bonded inside to support the centre of the chord, I'll try and remember to get a picture tomorow of a smashed one to explain what I mean.

I'm sure warren will be along soon to give advice, he has a lot of good advice when it comes to these
Edited 11 Years Ago by ajb100
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
ajb100 (19/03/2014)
Sorry, read blade as the end plates!

Havnt got a huge amount of experience with wings, but I've used the permabond adhesive from EC to join mine together.

I've done some repairs on F3 wings which use a support bonded inside to support the centre of the chord, I'll try and remember to get a picture tomorow of a smashed one to explain what I mean.

I'm sure warren will be along soon to give advice, he has a lot of good advice when it comes to these


Cheers man 
Wud b nice to see sum pics
Thanx
:-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search