Just be careful if it's been sitting around for awhile. It's very hygroscopic, and moisture kills it. So test it is still working after you apply it by using some masking tape or hot melt glue. If it's working then it will come off extremely easily. If you have a highly polished mould, you'll probably find that the tape won't even stick in the first place, it will just curl up on itself.
|