Hi I purchased some of your 2 part carbon epoxy to fill in the worn brake tract on my carbon wheels, and have realised that it has a low TG because when I brake the epoxy gets too hot and starts to burn away!!!!
Do you sell a epoxy that has a very high TG that comes in black and would be able to take the heat produced when braking.
Thanks

Colin gladstone  
Reply
Colinwhufc
Colinwhufc
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 7, Visits: 23
Also how long should I post cure it?
Thanks lads you've been a big help
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search