Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Fixing carbon bike wheel brake tract
Fixing carbon bike wheel brake tract
Post Reply
Like
2
Fixing carbon bike wheel brake tract
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Colinwhufc
Colinwhufc
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 23
Hi I purchased some of your 2 part carbon epoxy to fill in the worn brake tract on my carbon wheels, and have realised that it has a low TG because when I brake the epoxy gets too hot and starts to burn away!!!!
Do you sell a epoxy that has a very high TG that comes in black and would be able to take the heat produced when braking.
Thanks
Colin gladstone
Reply
Like
2
Reply
wozza
wozza
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Colinwhufc (18/03/2014)
What is post curing and how is it done , sorry for sounding thick !!
Post curing is reheating the part after the initial curing process at elevated temperatures. So if the resin is allowed to initially cure at ambient temperature say 20 Degrees C, the part is then placed in an oven or some other heat source and heated to a temperature above what the resin/part will be exposed to in use. So in your case if the temperature developed during braking is say 60 degrees then you need to post cure above that, say 70 degrees to include a safety margin. Hope that makes sense.
Warren
Carbon
Copies Ltd
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fixing carbon bike wheel brake tract
Colinwhufc
-
11 Years Ago
You would need to us our High Temperature Black Epoxy Skinning Basecoat which goes upto 180C....
Warren (Staff)
-
11 Years Ago
What is post curing and how is it done , sorry for sounding thick !!
Colinwhufc
-
11 Years Ago
[quote][b]Colinwhufc (18/03/2014)[/b][hr]What is post curing and how is it done , sorry for sounding...
wozza
-
11 Years Ago
Cheers warren . I just have to figure out where to find a oven big enough for a pair of bike wheels...
Colinwhufc
-
11 Years Ago
Do you know your target temp? There are ways around needing an oven as such depending on temp. The...
ajb100
-
11 Years Ago
I suppose the hotter the better. Could I build something myself, if so what temp could I possibly...
Colinwhufc
-
11 Years Ago
[quote][b]Colinwhufc (18/03/2014)[/b][hr]I suppose the hotter the better. Could I build something...
wozza
-
11 Years Ago
Nice one warren. Thanks for the advice How long should I bake it for?
Colinwhufc
-
11 Years Ago
[quote][b]Colinwhufc (19/03/2014)[/b][hr]Nice one warren. Thanks for the advice[/quote] Your...
wozza
-
11 Years Ago
I'm in stanford le hope in essex
Colinwhufc
-
11 Years Ago
Also how long should I post cure it? Thanks lads you've been a big help
Colinwhufc
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search