Hi

 New to the forum so bare with me

 I am a woodturner and want to cast wood in resin , some of the wood is very porous and so need stabilising

 I have used polyurethane resin with very poor success,Would using infusing resin work in my case

 I have a pressure pot and I'm sure I can get a vacuum pump

 Any help is greatly appreciated
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
To stabilise wood you should try thinning epoxy resin with epoxy thinner and brushing it on the wood. It should soak in rather remain glossy on the surface.

You can also use a product called everdure which is also pretty much a thinned epoxy.

https://www.smartmarine.co.nz/products/maintenance-paint/paint-2-pot/50553/everdure-primer-2-pack-500ml-kit/details/




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search