I fancy having a play with these out of autoclave pre-pregs.  The problem I have is that all my moulds are polyester based.  I've seen mention of pre-pregs that can be cured at 60'C.  Can anyone point me in the right direction for something suitable and perhaps comment on how they found them to use.  Thanks all.
Chenn
Chenn
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 10, Visits: 191
Surely any LTM material.. Standard 200g for visual and a 600g heavy depends what your making but these can be cured in an oven

Instagram - C14ENN
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Advanced Composites/Umeco VTM 264 has 65 degree C cure but the cook will take along time.

http://www.lavender-ce.com/wp-content/uploads/pds1154-vtm260-issue5.pdf




FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Magic, thanks!