I fancy having a play with these out of autoclave pre-pregs.  The problem I have is that all my moulds are polyester based.  I've seen mention of pre-pregs that can be cured at 60'C.  Can anyone point me in the right direction for something suitable and perhaps comment on how they found them to use.  Thanks all.
By FLD - 3/22/2014 9:44:29 PM

Magic, thanks!