Polyester resin with powder bound csm?


Author
Message
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Powder bound CSM works fine with polyester, so if you already have some then give it a go. Personally I don't particularly like the stuff, I find it a bit harder to work with than emulsion bound strand matt.
dbcrx
dbcrx
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
I'm thinking of getting me some polyester resin (normally only use epoxy) for playing with some small moulds and parts (non structural). I already have powder bound csm for use with epoxy - does polyester work ok with this or would I be better getting some emulsion bound?