By dbcrx - 2/18/2014 9:13:07 PM
I'm thinking of getting me some polyester resin (normally only use epoxy) for playing with some small moulds and parts (non structural). I already have powder bound csm for use with epoxy - does polyester work ok with this or would I be better getting some emulsion bound?
|
By Hanaldo - 2/20/2014 7:34:40 AM
Powder bound CSM works fine with polyester, so if you already have some then give it a go. Personally I don't particularly like the stuff, I find it a bit harder to work with than emulsion bound strand matt.
|
|