Hi:

I want to make a hollow tube for an aerobar shaped lik " _/ "

I was thinking on making it with an inflatable blader and a epoxy mould sliced in 2.

What do you recomend?
MAVERICK
MAVERICK
Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)Supreme Being (417 reputation)
Group: Forum Members
Posts: 27, Visits: 39
Hey Sergio,

I've heard on here somwhere that somebody have used RTV silicone for this sort of job, I think the idea is that you would make your split mould then fill it solid with silicone. then remove this from the mould after it has cured and wrap it with carbon (I bet the carbon fibre braided sleeve would be great for your job) when you clamp this into the mould you put it into an oven and the silicone expands with heat putting pressure on the laminate. For an inflatable bladder you could use a latex bike inner tube... you would need to cap the ends though, and make sure your mould was tough otherwise it'd go bang in a big way!
mhdghoul
mhdghoul
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 49, Visits: 113
at ec they have tubes from cf with many diameters u can cut it and attatch it angled the way you want and stiff it from inside and out side too

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
ant...
ant...
Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)Supreme Being (237 reputation)
Group: Forum Members
Posts: 17, Visits: 92
MAVERICK (13/03/2012)
Hey Sergio,

I've heard on here somwhere that somebody have used RTV silicone for this sort of job, I think the idea is that you would make your split mould then fill it solid with silicone. then remove this from the mould after it has cured and wrap it with carbon (I bet the carbon fibre braided sleeve would be great for your job) when you clamp this into the mould you put it into an oven and the silicone expands with heat putting pressure on the laminate. For an inflatable bladder you could use a latex bike inner tube... you would need to cap the ends though, and make sure your mould was tough otherwise it'd go bang in a big way!




Maverick - I like this idea, im gonna try this one day.  If you were making a tube though, how would you get the silicone out?

mhdgoul's idea seems best for this situation IMO, making tubes that look nice and straight is a pain.  

Id like to know where you could get the equipment to make your own inflatable bladers though???
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi,

I'm planning to do the same kind of stuff but on an easier scale, just for testing the technique...
This is the way I think i will do it:

I've ordered the Carbon braided sleeve 10mm a few days ago and the shipment will arrive tomorrow I think

1. I'll go get a PVC-tube, and cut it in halve
2. apply mouldrelease on both halves
3. Put an innertube of a bikewheel on the inside of the Carbon Fiber braided sleeve (also with lots of mouldrelease)
4. Coat the Sleeve with epoxy 
5. Close the 2 PVC-tubes with some ductape I guess 
6. Inflate with some compressed air
7. Let it cure

If possible I will pick something other than PVC so I could maybe put it in an oven to cure it with some heat.



Any remarks guys?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




jim
jim
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 1, Visits: 3
babolat uses prepreg carbon in an aluminum halved mold. they roll the precise layers of prepreg into this mold and then they pressurize the mold to push the carbon out into the mold. then they send it into the oven. the raquets come out precise every time. i'm not sure you can improve this engineeing, but if you have any ideas, i'd sure like to see them. 
Edited 14 Years Ago by jim
Manu
Manu
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 23, Visits: 435
hello! I also want to make carbon tube, in my case the most important is the lowest cost, my method will be the next, impregnated with epoxy a piece of carbon fiber cloth in a plane, allow it to reach its gel state, and use it as a pre-preg. Once I have this wrap it inan aluminum tube with mold release this tube is placed in a mold that I made properly to have the outer diameter desire and finally a curing oven. Once fully cured, with a slightblow to the aluminum tube that goes inside the carbon tube and ready to make more tubes!

www.ktuning.es  



https://www.facebook.com/Ktuning.es/ 


www.carboncycleparts.com 


https://www.facebook.com/CarbonCycleParts/
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Yes, EC do you have any contacts with materials for making bladers?

Ant, the silicone can be removed because it is cut up like a puzzle,
it fits together but you can remove it piece by piece from one end of tube.
This is how BST make CF wheels for motorcycles, they claim to have a patent for the method.
H4RTM4N
H4RTM4N
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 7, Visits: 203
Hey guys,

This is a very interesting post. I want to make a long, hollow CF/EP tube to record with my GoPro. I could use an aluminum tube to make a half-mould. From there, I would make two halves and then glue them together. However, the joint would be visible and the tube wouldn't be as strong as a hollow, one-piece CF/EP tube. 

Using an Inflatable Bladder would certainly be the best idea. I carried out some research and I found some interesting videos/posts from a very clever guy that makes his own R/C planes.

Making an Inflation Bladder for Assisted Composite Part Fabrication

https://vimeo.com/10665397

Layup of The Wyoming Wind Works DLG Fuselage

https://vimeo.com/35648020

Demolding of the Wyoming Wind Works DLG Fuse

https://vimeo.com/37883424

I still don't understand how putting reinforcements and resin in each side of the mould separately ends up in a solid piece when the mould is closed. There has to be some overlapping that the bladder is pressing against the mould or another clever solution. Trying to find and answer to this, I found this interesting post:

Closed-Mold Vacuum Infusion with a Bladder

http://www.rcgroups.com/forums/showthread.php?t=1594856

Another way of doing this seems to be the following:
  1. Make the two-halves independently using joggle tools in each mould.
  2. Apply glue to the edges while the parts are still in the moulds.
  3. Close the moulds and apply pressure.
Check this post for more detailed information: http://www.rcgroups.com/forums/showpost.php?p=11804764&postcount=135

Has any of you guys made a one-piece hollow part using any of these techniques? I'm seeking for advice because I'm very new to this. 
Zebra
Zebra
Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)
Group: Forum Members
Posts: 14, Visits: 32
For simple shapes like a tube, you could use a regular long balloon as your inflatable bladder. You won't even need a compressor. You just blow up the ballon inside the tube cavity until there is enough pressure. The. Pop it when it's cured.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search