Hi
 Can somebody explain me what is surfacing film? Is it one side impregnated prepreg or something else?
Cheers
combustioncraig
combustioncraig
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 26, Visits: 46
surface film refers to prepreg that is generally only used for the first layer.  It is in general more resin rich and has a lot of resin on one side of the prepreg.  This done because because you need more resin than normal to get a perfect class A surface finish.  If you were to use a regular prepreg that is not intented to be used as a surface layer then you morethan likely will have a pin hole resin stared surface finish.  I hope that answers your questions.   
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
Cheers :-)