For out of autoclave use:-

The Uni-mould specifications say it is suitable for pre-pregs up to 90 degrees C.

The Pre-preg guide suggests a cure temperature of 100 degrees C for 8 hrs.

So what system can be used for creating a mould when hoping to use pre-preg?

Many thanks for your advice on what I recognise is a basic question.