Whats the black thing on the white heater? In ur last pic. Do u use only 1 external heater blower?
roger sbk composites
roger sbk composites
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 17, Visits: 163
the black thing is a second heater as that 1500 watt max temp was 60c constant running so i added the second one and now they both come on on and of.... 



morepower i actualy purchased this one wich has two and wireless also.. check you pm
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
roger sbk composites (22/02/2014)
the black thing is a second heater as that 1500 watt max temp was 60c constant running so i added the second one and now they both come on on and of.... 



morepower i actualy purchased this one wich has two and wireless also.. check you pm
http://www.ebay.com/itm/131102947836?ssPageName=STRK:MEWNX:IT&_trksid=p3984.m1439.l2649

and i also purcahsed 6 of these
to mount in a box and be able to know the temp of all the molds in there

I see u used mdf boards, are u using any insulation to keep temp? Or just closed mdf box?
Im in the process of moving to prepreg as i have found awesomely cheap ooa prepreg here in turkey which they claim the results are pinholefree in oven only prepregs. May be i can getaway without getting an autoclave. (Altho i have quote for autoclave £500 yes 5 hundred quid without the heating elements, its a 500 litre and will be made from 8mm thick steel) so how big is ur oven? How long does it takes to get the relevant temp? Sorry for loads of question :-)
Regards
roger sbk composites
roger sbk composites
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 17, Visits: 163
No problem let go on pm