Part made by resin infusion
Part made by resin infusion
Post Reply
Like
9
Part made by resin infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Djekouk
Djekouk
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 30,
Visits: 987
Just wanted to show a part made by resin infusion. Original part and carbon replica :-)
Attachments
image.jpg
(
1K views,
2.00 MB
)
image.jpg
(
1K views,
1.00 MB
)
Tags
car part
carbon
Resin infusion
twill
Reply
Like
9
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
looks good!
Can you show the mold and how you managed to get the mount location ?
Reply
Like
10
Djekouk
Djekouk
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 30,
Visits: 987
20_rc51_00 (20/01/2014)
looks good!
Can you show the mold and how you managed to get the mount location ?
Cheers, doin the molds again as they were damaged, when molds ready will put a pic.
Put sum maskin tape behind the holes and put sum modelling clay on top, after demold i cut the holes with dremel.
Reply
Like
9
gambler99
gambler99
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 62
good
how to do a gloss surface finish ?
Reply
Like
11
Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Practice.
And watch the tutorial video, there's a lot of good tips in there. Nothing like seeing it done to get a feel for it!
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search