Kind of forget of this post, here is an update with the video of the silicone re-usable bag that was uploaded last week. Still some improvements to be made but learned a lot out of this one!


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




combustioncraig
combustioncraig
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 26, Visits: 46
Like matt said that RVB (reusable vacuum bags) are a great option but are a little tricky to make there is a steep learning curve that can be challenging.  Also RVB in general react with epoxy resin so they are sometimes limited to less than 50 runs (prepreg is easier on the bags then RTM). At boeing silicone vacuum bags are used extensively for debulking the parts but then regular vacuum bags are used or even double bagged on high investment products for actually making parts (they do this due to vacuum seal quality of RVB but I don't think any of us are on that level).  I would love to hear from someone on here that was able to get a good seal and nice finish with RVB.  I have always wanted to try it as it would save a lot money on my prepreg parts but I haven't personally taken the plunge.     
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I did, you can find some images and a video on my Facebookpage...

Image https://www.facebook.com/photo.php?fbid=340982672711711&set=a.227227080753938.1073741830.223877301088916&type=1&theater

Video https://www.facebook.com/photo.php?v=338377539638891&set=vb.223877301088916&type=2&theater


The video upload on youtube will be in around 3 weeks Smile

Here is a trailer of what to come in the following weeks on my youtubechannel
Part 1 and 2 are allready online Wink new upload every wednesday at 18:00 belgian time

still have to do some improvements and engineering on the bag but I will get there

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




RUSSO
RUSSO
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 4, Visits: 778
I've been doing a bit of research on the net and came across this silicone rubber vacuum bagging and thought it looked quite good as it seems to do away with gum tape, bagging material and waste as it's reusable. Anyone used anything like it before?

Silicone bagging
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search