Sdb
Sdb
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 5
Anybody know of a stockist of 2x2 glass in prepreg form? I'm fairly flexible on cloth weight, so long as it's under 300gsm.
Thanks in advance,
Steve
Reply
Like
2
morepower
morepower
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
Try SHD composites.. They will do it but you may have to order 10meters or more..
http://www.shdcomposites.com/
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search