That part was wet lay up vacuum bagged,layers 5 and additional 2 around mounting points. 
Jdmleesy
Jdmleesy
Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)
Group: Forum Members
Posts: 39, Visits: 380
Nice work what process do u use and how many layers?
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search