clio cover 4 years old
http://www.talkcomposites.com/Topic8948.aspx
By Shaneer22
-
12/28/2013 12:23:19 AM
https://www.dropbox.com/s/s98rdglcxzxuqar/photo-2.JPG
By Shaneer22
-
12/29/2013 8:43:41 PM
That part was wet lay up vacuum bagged,layers 5 and additional 2 around mounting points.