Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Making tabs/brackets
Making tabs/brackets
Post Reply
Like
3
Making tabs/brackets
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Zero Mass Motorsports
Zero Mass Motorsports
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 59
You could pre-make the mounting tabs ( wet lay-up over angle aluminum as the form copy)....and then later, Infuse them in your dry stack with additional fabric pre-cut to surround them for added flex and strength.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I would do the same as ajb100,
Don't think it is possible to mould them, and mould the brackets into the mould...
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
There's two ways to make mounting tabs. You can either make them from aluminium or carbon fibre/glass and then bond them on after either with adhesive or wet lay fabric on top.
Reply
Like
3
Munkee
Munkee
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 200
Hi all,
I'm new to the site and just getting the resolve to finally go ahead and make some c/f parts after years of wanting to give it a go.
I want to make a few bits for my motorbike and westfield and am in the stages of doing research on the various techniques needed.
How would I best go about tackling tabs/brackets that are moulded into some of the plastic parts on my bike? A case in point would be the back of the head light surround, which I've attached pics of (hopefully!) to show an example. Its to the best pic in the world. And the light unit is in 2 parts (black and silver plastic) but there are various tabs, brackets and screw holes to be tackled.
Any advice greatly received!
Cheers
Steve
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search