Problems when skinning interior lists BMW


Author
Message
t3c
t3c
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 1, Visits: 12
Hey guys,

This is my latest work. This is after 1 layer of base coat, then waiting 3 - 4 hours then apply the fabric. Let it fully cure.
Then I added 2 layers before I started to sand with 120 grit.

Now the problem I have is I sand through the carbon showing gaps where you can see through the epoxy.

My question is what am I doing wrong?


Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I guess you answered your question yourself...you are sanding through the CF.
120 is a very low number to start sanding with...I would mostly start with a 600 and go up till 2000.
If you think you are sanding to close to the CF at the end, just add a new layer of resin and repeat till perfect

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO