Hi I am fairly new to carbon skinning , I've done a few bits with good results , however  I would like to skin my speedo surround on my car , picture attached , I'm struggling to get it right , i'm using the 2x2 twill pro carbon from carbon mods so I know it's good stuff, any pointers would be great , main problem i am getting is ,I seem to get a crease in it as i am applying , do I need to do it in two stages or is just me not doing something right.
Thankyou
Attachments
speedo.jpg (301 views, 5.00 KB)
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You may well need to use more cut lines to prevent the creases.  You may even be able to cut out a small triangle shape in places so that the carbon edges meet without overlap.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search