By pauldee - 12/10/2013 12:47:52 AM

Hi I am fairly new to carbon skinning , I've done a few bits with good results , however  I would like to skin my speedo surround on my car , picture attached , I'm struggling to get it right , i'm using the 2x2 twill pro carbon from carbon mods so I know it's good stuff, any pointers would be great , main problem i am getting is ,I seem to get a crease in it as i am applying , do I need to do it in two stages or is just me not doing something right.
Thankyou
By Warren (Staff) - 12/10/2013 9:26:39 AM

You may well need to use more cut lines to prevent the creases.  You may even be able to cut out a small triangle shape in places so that the carbon edges meet without overlap.