I would go for 5 layers on this part.. Soric in the middle, then E-Glass, then outer layer of CF.  No print-through from the Soric, nice and stiff.  Edges made with either enough layers of CF to match the Soric, or CF tape.
 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Jdmleesy
Jdmleesy
Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)
Group: Forum Members
Posts: 39, Visits: 380
I was originally thinking of 200g cf/soric/200g cf it was just the print thru that people talk about that put me off but I do like the idea of having the part that thick

Thanks for the advise m8
 
dbcrx
dbcrx
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
if you want it to fit nice and work, wouldn't you have to make it the same thickness as the original? in which case you'll want some sort of core material instead of the glass.
Jdmleesy
Jdmleesy
Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)
Group: Forum Members
Posts: 39, Visits: 380
Thanks for the help people
Jdmleesy
Jdmleesy
Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)Supreme Being (279 reputation)
Group: Forum Members
Posts: 39, Visits: 380
I'm getting parts 2gether to start making a sunroof bung for my car but I'm just struggling for what way to stack the materials because costs are low after buying all the equipment involed 

I want the part to look oem as possible so I can have it attached to the mechanism if I choose or just use it as a bung.
Iv seen some people using 
200g carbon then 3/4 layers of 200/300g woven glass would this be stiff enough like this?
If not what would be good enough amount if layers that's not 2 expensive? 
The part is 20"x30" and there will be a front and back mould that will need bonding together.

Thanks for any help
Daz
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search