Ok so I have resisted doing the tub as its a huge amount of work... Ive made moulds and composite panels for the Front & rear clams, doors and front wings.... I wrapped the roof and window panels on the Tub which looked ok but not perfect and there was clearly no benefit other than cosmetics and it never really sat right with me.... I felt I had left the car unfinished!

So I have striped the car completely, sent the engine for a check over (ready for more power next year) and have been sanding the tub ready to start making the moulds.

Im not going to rush this project and I will need to make an oven to properly post cure it... Im also overseas with work around 5 weeks over the next few months so progress will be slow... but i will try to update this thread with picks to show process/progress.







roof is carbon wrapped with a v weave... its not perfect and didn't save weight.

Edited 13 Years Ago by andygtt
ajb100
ajb100
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Always been impressed with you and this car, not failing to do it again here either!
FLD
FLD
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
As above for me.  Carbon tub.....mentalist!  I'm really looking forward to seeing this one.  Its an amazing project.
Matthieu Libeert
Matthieu Libeert
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
looking forward to follow your project Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Warren (Staff)
Warren (Staff)
Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Youve got the same idea as me!! Should be awesome when done.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
wojtepanik
wojtepanik
Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)Supreme Being (809 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Hi
So you are doing something like monocoque? because I am not sure what more can be done here with carbon Tongue maybe wheels BigGrin

~~~Everytime I hear sound of demoulding part I have eargasm~~~
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
wojtepanik (10/12/2013)
Hi
So you are doing something like monocoque? because I am not sure what more can be done here with carbon Tongue maybe wheels BigGrin


I started making the moulds for my carbon seats a few weeks back, also made a diffuser which is nearly finished.... so there is always things left to make from carbon.

However Im not sure my composite skills are up to making wheels lol
FLD
FLD
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
How about a sump or cam covers etc?
Warren (Staff)
Warren (Staff)
Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Ive looked into doing cam covers before. It all depends on the Oil sealing arrangements on the underside.  To get a nice cosmetic smooth upper, you may sacrifice a smooth lower if you want to keep a simple one sided mould. 

However you can skim a flat face onto the bottom of the carbon if you make it oversize.  If the internal oil detailing is complex you can make an inner and outer mould, 2 carbon parts then bond together.

Obviously a suitable temperature resin system is a must.

In my opinion you would also be wise to incorporate a layer of kevlar in the layup to prevent any cracking issues with heat cycling or potential burst issue with a thin camcover if you have a heavily pressurised crankcase due to a breathing issue.

Sumps I would be concerned about the consequences of a minor impact, even with kevlar when compared to metal sumps.  Many metal sumps will just dent or crack thus avoiding any catastrophic instant oil loss.  However a composites one would likely cave in and maybe hole but at least have lots of cracks.

Also permenant immersion in engine oil and combustion products would be a challenging environment for the carbon/epoxy to survive.  You may need a inside coating or different resin lining. Vinylester resins have a very high chemical resistance to oils and petroleum based products so may be the solution for chemical resistance.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 13 Years Ago by Warren (Staff)
FLD
FLD
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thats interesting detail Warren.  Always appreciate your knowledge Smile