Rick Lloyd
Rick Lloyd
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 20
Can any one tell me what the max. thickness that can be infused at one time
I need to have a total thickness of 10mm
can this be done in one shot
It is all going to be fibreglass and the layup is going to be
2x 80 gram
2x 200 gram
2x 300 gram 90 def
2x 300 gram 45deg
2x 300 gram 90 def
2x 300 gram 90 def
2x 300 gram 45deg
2x 300 gram 45deg
until 10mm is reached and then
2x 80 gram
2x 200 gram
to balance the layup
is this possible any help would be great
Thanks
Rick
Edited
13 Years Ago by
Rick Lloyd
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Resin Infusion
Rick Lloyd
-
13 Years Ago
Hi! It depends on your resin specification, for ex. mine has max thickness of 12-15mm, check your...
wojtepanik
-
13 Years Ago
I have seen over 50mm infused (not done it myself but had it demonstrated) so as mentioned it...
ChrisR
-
13 Years Ago
As said it depends both on the material and the resin viscosity. With our IN2Epoxy Infusion Resin...
Warren (Staff)
-
13 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search