Gloss coat surface prep


Author
Message
cpkielycua
cpkielycua
Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)Supreme Being (229 reputation)
Group: Forum Members
Posts: 29, Visits: 285
Despite all my efforts I have not been able to get a pinhole free surface. The materials are great, and the closest I have come, but to date I have been unable to figure it out. 

That being said, for the time being, I will fill, sand and clear coat the surface. I have done this in the past and had some delamination of the 2 part auto UV clear coat. Is there any special surface prep required?  Do I need to sand to a certain grit, not too fine, not too coarse?  Is there a chemical prep of the surface to aid bonding?

Thanks
Chris
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search