posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 102,
Visits: 582
Hi !
I was talking with my supplier and he recommended me to use epoxy gelcoat to make moulds as it is better, stiffer etc. but if you use epoxy gelcoat you have to use epoxy resin and woven glass as a reinforcement so the price would be really high, so I started to think, we have in Poland epoxy resin called epidian 53 and it is normal epoxy but the catalyst/hardener contains styrine, so I though, that I could use epoxy gelcoat, epidian and as a reinforcement CSM. Epidian is really cheap, it coasts about 15 euro for 1kg with hardener. So guys, what do you think about doing mould like this? Will it work? Thanks for answer. Sorry for my enlish
Bye
Wojtek from Poland
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
2
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
€15 for a 1kg kit isn't "cheap". It's the cost of a standard epoxy. It sounds like you've got a modified epoxy vinyl ester, maybe not. Either way it seems to be a polish product which hasn't left the country.
You're better off using a tried and tested Vinyl Ester like Neogel or Nord GC206, followed by a rapid tooling system like Neomould or Optimold.
Reply
Like
3
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
carboncactus (09/11/2013)
€15 for a 1kg kit isn't "cheap". It's the cost of a standard epoxy.
Umm, 1,2 kg of west system 206 (a+b) costs 35 € so there is sense of using epidian ;(
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
3
gary051
gary051
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 1,
Visits: 9
hi will the parts being made from the mould be made from epoxy or poleyester?
Reply
Like
3
Zorongo
Zorongo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 40,
Visits: 330
styrene from resin/hardener will solve the polyestyrene foam if in direct contact.
Epoxy gel coat will créate a barrier between foam and laminating resin. It will work if it doesn't content styrene.
So.... make a test and you´ll know from first hand...
Epoxy + mat should work OK. Slower impregnation so, a bit of patience, and maybe a Little bit thicker mould, if it will withstand vacuum, high pressure or high temperatura.....
Edited
12 Years Ago by
Zorongo
Reply
Like
2
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
why not just use a powder based CSM suitable for use with epoxy?
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I always use a vinylester. It's fast, cheap, chemical/heat resistent and works well with epoxy and polyester parts
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search