Hello...

My vacuum pump is a big one..

Free Air Displacement 40 m3/hour..

Do i need to slow it down?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

No, the Free Air Displacement of a vacuum pump will make no difference to the speed of an infusion whatsoever. The only thing that affects the speed of an infusion is the level of vacuum (the vacuum pressure) and since infusions should always be done at 100% vacuum the only problem is whether your vacuum pump is pulling enough vacuum, not whether you need to slow it down.

Check your pump with an accurate gauge. You should be pulling 100% / -1bar. If you've got that (not close but actually reading a full -1bar) then you should be fine.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
batbyggare
batbyggare
Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)
Group: Forum Members
Posts: 18, Visits: 142
Okej, thats good.

Yes it manage 100% vacuum.

Thanks again..
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search