Hi

We had purchased this pump off you less than 6 months ago. This morning we witnessed oil leaking through the pump and vacuum hoses onto the through-bag connectors. There is also oil leaking off the glass around the oil level indicator on the pump. Could you advise me what can be done in order to get it reapired at the earliest opportunity. Does Easy COmposites have a provision for repairing pumps? This has now stopped production and therefore demand s immediate attention.

Many thanks

Mohammed 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search