Gel coat issues with easy-lease for fibreglass wet lay up
Gel coat issues with easy-lease for fibreglass wet lay up
Post Reply
Like
2
Gel coat issues with easy-lease for fibreglass wet lay up
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Maxirally
Maxirally
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 47
Hi, I have recently purchased some of your chemical release agent and am having some issues getting the gel coat to lie in the mould properly. It appears to be repelling in areas and I am having to keep rebrushing to ensure complete coverage.
In it's self this is not an issue, however I am concerned this reworking of the gel coat is causing the 'alligatoring' issues I am experiencing.
I have followed the product instructions, used the mould cleaner, and applied 4 coats of easy-lease 24 hours prior to lay-up.
Have you any suggestion as to what I may be doing wrong please?
Many thanks, Tony
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Gel coat issues with easy-lease for fibreglass wet lay up
Maxirally
-
12 Years Ago
You are not doing anything wrong. Easylease makes such a repellant surface that often any steep...
Warren (Staff)
-
12 Years Ago
When putting on a coat of wax would this have to be polished off as normal, Would it remove the...
Boat Planter
-
12 Years Ago
The wax is lightly buffed as normal. For reapplication the Easylease is loaded in solvants anyway...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search